Compounded PP-FR-V0 PP
Compounded · PP-FR-V0

Compounded PP-FR-V0 PP

Melt index: 14 g/10min @230°C/2.16kg Density: 1.2 g/cm³ Tensile strength: 28 MPa

Electrical housing, socket, battery case

Chat on WhatsApp  Send inquiry

Technical data

Melt index14 g/10min @230°C/2.16kg
Density1.2 g/cm³
Tensile strength28 MPa
Izod impact5 kJ/m²
HDT120 °C
Vicat148 °C

Full TDS / MSDS / COA available on request.