[email protected]

← Kembali ke daftar produk

DuPont 500P POM
DuPont · 500P

DuPont 500P POM

Melt index: 14 g/10min @190°C/2.16kg Density: 1.42 g/cm³ Tensile strength: 68 MPa

Precision gear, bearing, automotive part

Chat WhatsApp  Kirim permintaan

Technical data

Melt index14 g/10min @190°C/2.16kg
Density1.42 g/cm³
Tensile strength68 MPa
Izod impact7.5 kJ/m²
HDT115 °C
Vicat160 °C

Full TDS / MSDS / COA available on request.

Lihat produk

Permintaan

Kirim kebutuhan Anda

WhatsApp+8615268436369
Chat WhatsApp